Secondary Fibres to get quality de-inked pulp.
Wet Strenght laminated papers.
Virgin pulp.
Batch operation at consistency 12 - 20 % depending on the furnish. For Dumping high consistency pulper to remove plastics/ other wt contaminant without cutting it.
Rotor Mounted on bearing Body and Belt Drive System with flat pulleys.
Bearing body is bolted with vat.
Vat is supported on 3 to 4 legs.
VAT Contains 3 nos to 4 nos. baffles and bottom shaped for optimal circulation.
Discharge hole is equipped with pneumatic pulp valve.
Reduction in pulping time.
Less power consumption in comparision with traditional pulping ( 30 KWH/ton ).
No Cutting of contaminents.
Low residual flake contents.
low residual flake contents.
Low residual stickies contents. .
HHCP-4 -- 4 MQU -- 90 -- 120
HHCP-6 -- 6 MQU -- 110 -- 150
HHCP-8 -- 8 MQU -- 150 -- 200
HHCP-12 --12 MQU --230 -- 300
HHCP-16 --16 MQU --300 -- 400